UNS DesignationB | TypeB | Carbon | Manganese | Phosphorus | Sulfur | Silicon | Chromium | Nickel | Molybdenum | Nitrogen | Other Elements |
---|---|---|---|---|---|---|---|---|---|---|---|
Duplex (Ferritic-Austenitic) Grades | |||||||||||
S32760 | -- | 0.030 | 1.00 | 0.030 | 0.010 | 1.00 | 24.0-26.0 | 6.0-8.0 | 3.0-4.0 | 0.20-0.30 | Cu 0.50-1.00, W 0.50-1.00, %Cr+3.3x%Mo +16x%N≥40 |
A. Maximum or range unless otherwise indicated.
B. See Guide A959/A959M.
UNS Designation | Solution Temperature, °F [°C] B,C | Size Range | Mechanical Properties | ||||
---|---|---|---|---|---|---|---|
Tensile Strength, ksi [MPA] | Yield Strength, ksi [MPA] | Elongation in 2” [50 mm] or 4D % | HardnessD | ||||
Rockwell, HRC maximum | Brinell, maximum | ||||||
S32760 | 2010 [1100] | -- | 109 (750] | 80 [550] | 25 | 30 | 290 |
A. Values shown are minimums or ranges unless maximum is indicated.
B. ± 25°F [15°C].
C. Quenched in water.
D. Either Rockwell or Brinell testing is permitted unless thickness is below 1⁄2 ” in which
case Rockwell is preferred.
UNS Designation | Type | Condition | Grade Symbol |
---|---|---|---|
Duplex (Ferritic-Austenitic) Grade | |||
S32760 | -- | -- | 32760 |