UNS DesignationB | TypeB | Carbon | Manganese | Phosphorus | Sulfur | Silicon | Chromium | Nickel | Molybdenum | Nitrogen | Other Elements |
---|---|---|---|---|---|---|---|---|---|---|---|
Duplex (Ferritic-Austenitic) Grades | |||||||||||
S32750 | 2507 | 0.030 | 1.20 | 0.035 | 0.020 | 0.80 | 24.0-26.0 | 6.0-8.0 | 3.0-5.0 | 0.24-0.32 | Cu 0.50 |
A. Maximum or range unless otherwise indicated.
B. See Guide A959/A959M.
UNS Designation | Solution Temperature, °F [°C] B,C | Size Range | Mechanical Properties | ||||
---|---|---|---|---|---|---|---|
Tensile Strength, ksi [MPA] | Yield Strength, ksi [MPA] | Elongation in 2” [50 mm] or 4D % | HardnessD | ||||
Rockwell, HRC maximum | Brinell, maximum | ||||||
S32750 | 1880 - 2060 [1025 - 1125] |
2 in. and under | 116[800] | 80 [550] | 15 | 33 | 310 |
A. Values shown are minimums or ranges unless maximum is indicated.
B. ± 25°F [15°C].
C. Quenched in water.
D. Either Rockwell or Brinell testing is permitted unless thickness is below 1⁄2 ” in which
case Rockwell is preferred.
UNS Designation | Type | Condition | Grade Symbol |
---|---|---|---|
Duplex (Ferritic-Austenitic) Grade | |||
S32750 | 2507 | -- | 32750 |